By Welding - You should use an alloy with low silver content, to meet the brass color. Fusion temperature close to 700-800°C. Cleaning and repolishing may lead to a tougher job.
By Butting - If the job is made properly, this will look like a hair lying down on the handrail. To meet this target, two critical issues have to be solved; a precise length cutting and sharp ends. Polishing makes the edges round. To avoid that, you can add a short piece at the end of the handrail and remove it when completed.